Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2500 - 2900 cP | 2500 - 2900 cP | Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-40/27 Polycaprolactone based TPU Pearlstick 45-40/27 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility:.. |
|||
Brookfield Viscosity | 2500 cP | 2500 cP | 15% NV at MEK, SPDL No 3, 10 rpm; SRTM 3032-2-S |
Lubrizol Estane® UB450 Thermoplastic Polyurethane Type: Estane® UB450 is a Shore A, polyester based, solvent-borne adhesive thermoplastic polyurethane (TPU).Uses: Solvent Coating.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Brookfield Viscosity | 2500 cP @Temperature -40.0 °C |
2500 cP @Temperature -40.0 °F |
ASTM D2983 |
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Brookfield Viscosity | 2500 - 2900 cP @Temperature 25.0 °C |
2500 - 2900 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 200 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 200: Tack-free and h.. |
|||
Brookfield Viscosity | 2500 - 4000 cP | 2500 - 4000 cP | RVT #3 sp @ 20 rpm |
3M Scotch-Weld™ TL43 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Brookfield Viscosity | 2500 - 5000 cP | 2500 - 5000 cP | RVF #4 sp @ 20 rpm @ 62°C |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |
|||
Brookfield Viscosity | 2500 - 4500 cP @Temperature 191 °C |
2500 - 4500 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive Same as 6111 but has higher heat resistance and blue in colorInformation provided by 3M |
|||
Brookfield Viscosity | 2500 - 4500 cP @Temperature 191 °C |
2500 - 4500 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 6111HT Tan Bulk only Adhesive Same as 6111 but has higher heat resistanceInformation provided by 3M |
|||
Brookfield Viscosity | 2500 cP | 2500 cP | |
BCC Products BC 8660E Urethane Elastomer BC8660E is a multi-purpose elastomer that can perform many functions. Special product characteristics are: excellent use for molds for casting of concrete and plaster, resists moisture absorption, d.. |
|||
Brookfield Viscosity | 2500 cP @Temperature 23.9 °C |
2500 cP @Temperature 75.0 °F |
mixed |
BCC Products BC 8690E Polyurethane Elastomer BC 8690E is a two-component urethane elastomer compound specifically designed for casting applications. This product is a safe, easy-to-handle, room temperature mixing and curing system that contain.. |