3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Same as 6111 but has higher heat resistance and blue in colorInformation provided by 3M
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Brookfield Viscosity 2500 - 4500 cP

@Temperature 191 °C
2500 - 4500 cP

@Temperature 375 °F
Mechanical Properties Metric English Comments
Peel Strength 0.614 kN/m
3.50 pli
HDPE, 180°
2.52 kN/m
14.4 pli
PP, 180°
2.86 kN/m
16.3 pli
PVC, 180°
2.89 kN/m
16.5 pli
ABS, 180°
4.49 kN/m
25.6 pli
Fir, 180°
4.56 kN/m
26.0 pli
on canvas
5.24 kN/m
29.9 pli
Cold Rolled Steel, 180°
Thermal Properties Metric English Comments
Flash Point 276 °C
529 °F
Ring & Ball Softening Point 107 °C
225 °F
ASTM E28-99
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month