Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 0.77 cP | 0.77 cP | Toluene sol., 25% wt; ASTM D1084 |
Polimeri Europa Europrene® SOL T 6205 Styrene - Butadiene Block Copolymer Europrene® SOL T 6205 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 25% weight and diblock content is 15%. .. |