Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 11400 cP @Temperature -40.0 °C |
11400 cP @Temperature -40.0 °F |
|
ChevronTexaco Heavy Duty Synthetic Automatic Transmission Fluid Texaco Synthetic Automatic Transmission Fluid Heavy Duty delivers value through:Extended drains of up to four times that of a conventional automatic transmission fluid.Protection against the formati.. |
|||
Brookfield Viscosity | 11400 cP @Temperature -40.0 °C |
11400 cP @Temperature -40.0 °F |
|
ChevronTexaco Synthetic Automatic Transmission Fluid, Heavy Duty FeaturesChevron Synthetic Automatic Transmission Fluid Heavy Duty is engineered to meet the performance requirements of Allison TES 295 for severe duty and extended drain intervals. It is manufactu.. |