Polymer Property : Brookfield Viscosity = 12.96 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 12.96 cP

@Temperature 68.0 °C
12.96 cP

@Temperature 154 °F
The Chemical Company ChemFlexx™ DOA C22H42O4
Chemflexx DOA is a Dioctyl adipate (DOA) plasticizer. DOA is an ester of 2-ethylhexanol and adipic acid. It is a low-toxicity, biodegradable, light colored, oily liquid generally used as a plasticiz..