Polymer Property : Brookfield Viscosity = 1200 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 800 - 1200 cP

@Temperature 20.0 °C
800 - 1200 cP

@Temperature 68.0 °F
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A
Lubrizol Advanced Materials Pearlstick® 45-50/08 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 45-50/08 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-..
Brookfield Viscosity 400 - 1200 cP
400 - 1200 cP
#2/20 rpm
Mallard Creek Polymers BarrierPro® 4545 SBR Emulsion
BARRIER PRO® 4545 is an anionic carboxylated styrene-butadiene copolymer latex. Features: highly stable, good compatibility with fillers and pigments, etc., cured films are tough and pliable, cur..
Brookfield Viscosity 350 - 1200 cP
350 - 1200 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4305 SBR Latex
ROVENE® 4305 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This non-woven and textile binder offers outstanding..
Brookfield Viscosity 350 - 1200 cP
350 - 1200 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 5005 SBR Latex
ROVENE® 5005 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This paper saturant offers good water and solvent re..
Brookfield Viscosity 900 - 1200 cP
900 - 1200 cP
LVF Sp #2 @30 rpm
3M Scotch-Weld™ LO1000 Low Odor Instant Adhesive
3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o..