Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 7500 - 18000 cP | 7500 - 18000 cP | RVF #6 sp @ 20 rpm |
3M Scotch-Weld™ 4799 Industrial Adhesive 3M™ Scotch-Weld™ Industrial Adhesive 4799 can be used to bond most EPDM rubber, sponge rubber, rubber sheeting, felt, canvas, linoleum and other lightweight materials to many metals, woods, concre.. |