Physical Properties Metric English Comments
Brookfield Viscosity 180000 - 220000 cP

@Temperature 25.0 °C
180000 - 220000 cP

@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Lord Adhesives Metech 3524 Silver Conductor Composition
This silver conductor composition is designed for screen printing applications requiring nickel barrier plating. It fires to a highly dense film which is resistant to acidic plating solutions.All in..
Brookfield Viscosity 180000 - 220000 cP

@Temperature 25.0 °C
180000 - 220000 cP

@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Lord Adhesives Metech 3541 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..
Brookfield Viscosity 180000 - 220000 cP

@Temperature 25.0 °C
180000 - 220000 cP

@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Lord Adhesives Metech 3542 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..
Brookfield Viscosity 180000 - 220000 cP

@Temperature 25.0 °C
180000 - 220000 cP

@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Lord Adhesives Metech 3543 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..
Brookfield Viscosity 180000 - 220000 cP

@Temperature 25.0 °C
180000 - 220000 cP

@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Lord Adhesives Metech 3540 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..