Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1000 - 1900 cP @Temperature 25.0 °C |
1000 - 1900 cP @Temperature 77.0 °F |
20% Toluene solution; KM 06 |
Kraton® G1650 E (SEBS) Linear Block Copolymer Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i.. |