Physical Properties Metric English Comments
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 1rpm
Lord Adhesives 8601 Polymer Resistor Composition
LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord.
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 1rpm
Lord Adhesives 8611 Polymer Resistor Composition
LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord.
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 1rpm
Lord Adhesives 8621 Polymer Resistor Composition
LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord.
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 1rpm
Lord Adhesives 8631 Polymer Resistor Composition
LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord.
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 1rpm
Lord Adhesives 8641 Polymer Resistor Composition
LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord.
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 1rpm
Lord Adhesives 8651 Polymer Resistor Composition
LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord.
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 1rpm
Lord Adhesives 8661 Polymer Resistor Composition
LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord.
Brookfield Viscosity 20000 - 40000 cP

@Temperature 25.0 °C
20000 - 40000 cP

@Temperature 77.0 °F
RVT, Spindle #7 @ 20rpm
Lord Adhesives Metech 6103 Silver Conductor
This material is a low viscosity thermoplastic printing ink designed for general purpose application onto various rigid substrate compositions such as epoxy board or other rigid plastic. It is desig..
Brookfield Viscosity 20000 cP

@Temperature -40.0 °C
20000 cP

@Temperature -40.0 °F
ExxonMobil 75W-80 Mobilfluid LT
Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to..
Brookfield Viscosity 20000 - 30000 cP
20000 - 30000 cP
Zeon Test #170
Zeon Chemicals Nipol® 1312 Liquid Nitrile Elastomer
Nipol 1312 is a copolymer of butadiene and acrylonitrile with medium oil resistance in liquid form. Sufficient antioxidant is added during manufacture for normal storage conditions.Plasticizer used ..
Brookfield Viscosity 20000 cP

@Temperature -40.0 °C
20000 cP

@Temperature -40.0 °F
ExxonMobil 75W-80 Mobilfluid LT
Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to..
Brookfield Viscosity 20000 - 60000 cP
20000 - 60000 cP
RTV No. 7, 10 rpm
Dow BETAMATE™ 7000 fast curing polyurethane adhesive component
One component of a room temperature fast curing polyurethane structural adhesive.Information provided by Dow
Brookfield Viscosity 20000 - 60000 cP
20000 - 60000 cP
RTV No. 7, 10 rpm
Dow BETAMATE™ 7050 L Epoxy
One component of a room temperature fast curing polyurethane structural adhesive.Information provided by Dow
Brookfield Viscosity 20000 cP

@Temperature 23.9 °C
20000 cP

@Temperature 75.0 °F
Mixed
BCC Products BC 7009-1 Epoxy Casting
BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding exces..