Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1700 - 2200 cP @Temperature 20.0 °C |
1700 - 2200 cP @Temperature 68.0 °F |
Brookfield RVF sp. 6, 20 rpm solution at 15% in MEK; MQSA N° 40A |
Lubrizol Advanced Materials Pearlstick® 48-60/19 Linear Thermoplastic Polyurethane Elastomer Pearlstick 48-60/19 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.Solubility: Pearlstick 48-60.. |