Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 23.3 cP | 23.3 cP | One Day Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 180 Series 180X7 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 180X7 is low molecular weight homopolymer resin that provides good chemical foam characteristics with excellent overblow resistance. The modified rhelogy of Geon® 180X7 provides increased vi.. |