Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2385 cP @Temperature -18.0 °C |
2385 cP @Temperature -0.400 °F |
ASTM D2983 |
ExxonMobil 526 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Brookfield Viscosity | 2385 cP @Temperature -18.0 °C |
2385 cP @Temperature -0.400 °F |
ASTM D2983 |
ExxonMobil 526 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |