Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 240 cP @Temperature 200 °C |
240 cP @Temperature 392 °F |
Melt |
Zeon Chemicals Quintone® A100 Aliphatic Hydrocarbon Resin C5 type (piperylene precursor). General-purpose, suitable for adhesives based on natural rubberInformation provided by Zeon Chemicals L.P. |