Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3200 cP @Temperature 25.0 °C |
3200 cP @Temperature 77.0 °F |
Mixed |
BCC Products BC 5010 Epoxy Laminating System BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor.. |