Brookfield Viscosity 325 cP
325 cP
One Hour Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method
PolyOne Geon™ 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 174 is a medium molecular weight, fine particle size homopolymer dispersion resin. It provides a good balance of fused film properties and processing temperatures. It is recommended for appli..