Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 39000 - 56800 cP @Temperature 25.0 °C |
39000 - 56800 cP @Temperature 77.0 °F |
Spindle 6 @ 10rpm |
Lord Adhesives Circalokâ„¢ EP-937 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-937 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Brookfield Viscosity | 39000 cP @Temperature -40.0 °C |
39000 cP @Temperature -40.0 °F |
|
ChevronTexaco TEGRA® SAE 75W-90 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality, multipurpose gear lubricants.It is manufactured from synthesized hydrocarbon base fluids which have exceptional thermal and oxid.. |