Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 4.0 cP | 4.0 cP | One Day, V12, Geon® 1010 |
PolyOne Geon™ 210 Series 218 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol and or Fused Film Formulation F2 consists of 60 parts of Geon®178 + 40 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940 Note: Plastisol Formulation F1 consis.. |
|||
Brookfield Viscosity | 4.0 cP | 4.0 cP | One Day Viscosity @ 2rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 210 Series 215 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 215 is a low molecular weight particle size homopolymer blending resin intended for use in plastisol formulations. It improves air release performance resulting in reduced scrap rates. It dec.. |