Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3.10e+7 - 4.50e+7 cP @Temperature 25.0 °C |
3.10e+7 - 4.50e+7 cP @Temperature 77.0 °F |
6 rpm or 3 rpm depending on viscosity |
DuPont Performance Polymers Neoprene AC SOFT Polychloroprene Rubber
(discontinued **) Description: Chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development.Processing and Performance Features: Primary use is in contact adh.. |