Brookfield Viscosity 4.95 cP
4.95 cP
One Day Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
PolyOne Geon™ 170 Series Adept E 49 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Adept E49 is a low molecular weight homopolymer dispersion resins intended for use in variety of plastisol applications and processes. It reduces scrap rates and manufacturing costs by extend..
Brookfield Viscosity 4.95 cP
4.95 cP
Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method
PolyOne Geon™ 120 Series 124A Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 124A is low molecular weight resin providing lower gelation and faster fusion characteristics. It provideds good chemical foamability for producing medium to high density foams. It gives good..