Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 440 cP | 440 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone |
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane Features: Hard, flexible, abrasion resistant coatings. Primarily used for all solution binder for inks and lacquers on fabrics and various substrates.Uses: Adhesives and inks & lacquers, pigment bin.. |