Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 580 cP | 580 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4019 SBR Latex ROVENE® 4019 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external c.. |