Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 6.18 cP | 6.18 cP | One Day Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer) Geon® 136 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy saving and the ability to work with heat sensitive substrates. The .. |
|||
Brookfield Viscosity | 6.18 cP | 6.18 cP | One Day Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer) Geon® 138 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy savings and the ability to work with heat sensitive substrates. The.. |