Physical Properties Metric English Comments
Brookfield Viscosity 10 - 60 cP
10 - 60 cP
Spindle # 2, rpm 60
Michelman® Michem® Lube 723 Nonionic paraffin wax emulsion
Description: Nonionic paraffin wax emulsionUsage: Michem® Lube 723 provides excellent water repellancy, lubricity, release and wood end check protection when used in the paint and coatings indust..