Polymer Property : Brookfield Viscosity = 7.50e+7 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 5.40e+7 - 7.50e+7 cP

@Temperature 25.0 °C
5.40e+7 - 7.50e+7 cP

@Temperature 77.0 °F
6 rpm or 3 rpm depending on viscosity
DuPont Performance Polymers Neoprene AD-30 Polychloroprene Rubber  (discontinued **)
Description: Chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development. More color-stable than neoprene AC during storage.Processing and ..