Physical Properties Metric English Comments
Brookfield Viscosity 950000 - 1.60e+6 cP
950000 - 1.60e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-730 Class B-12 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Brookfield Viscosity 950000 - 1.60e+6 cP
950000 - 1.60e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-730 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Brookfield Viscosity 950000 - 1.60e+6 cP
950000 - 1.60e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-730 Class B-6 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Brookfield Viscosity 950000 - 1.30e+6 cP
950000 - 1.30e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-770 Class B-1 Aerospace Sealant
3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio..
Brookfield Viscosity 950000 - 1.30e+6 cP
950000 - 1.30e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-770 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio..
Brookfield Viscosity 950000 - 1.60e+6 cP
950000 - 1.60e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-730 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..