Physical Properties Metric English Comments
One Hour Half Life Temperature 110 °C
230 °F
Akzo Nobel Trigonox® C-50D-pd Peroxide Cure Agent
Trigonox C-50D-pd is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural rubber and synthetic rubbers. Chemical Description: tert-Butyl peroxybenzoate, pow..
One Hour Half Life Temperature 110 °C
230 °F
Akzo Nobel Trigonox® C-40B-pd Peroxide Cure Agent
Trigonox C-40B-pd is a monofunctional peroxide which is used for the crosslinking of organic rubbers and silicone rubbers.Chemical Description: tert-Butyl peroxybenzoate, powder, 40% with inert fill..