One Hour Half Life Temperature 63.0 °C
145 °F
Akzo Nobel Trigonox® SBP Polymerization Initiator
Initiator for the (co)polymerization of ethylene, vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonateCAS Number: 19910-65-7Acronym: SBP; Tx SBPInformation provid..
One Hour Half Life Temperature 63.0 °C
145 °F
Akzo Nobel Trigonox® SBP-C30 Polymerization Initiator
Initiator for the (co)polymerization of ethylene, vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonate, 30% solution in odorless mineral spiritsCAS Number: 19910-..
One Hour Half Life Temperature 63.0 °C
145 °F
Akzo Nobel Trigonox® SBP-C60 Polymerization Initiator
Initiator for the (co)polymerization of ethylene, vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonate, 60% solution in odorless mineral spiritsCAS Number: 19910-..
One Hour Half Life Temperature 63.0 °C
145 °F
Akzo Nobel Trigonox® SBPS Polymerization Initiator
Initiator for the (co)polymerization of vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonateCAS Number: 19910-65-7Acronym: SBP; Tx SBPInformation provided by Akzo..
One Hour Half Life Temperature 63.0 °C
145 °F
Akzo Nobel Trigonox® SBPS-C60 Polymerization Initiator
Initiator for the (co)polymerization of vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonate, 60% solution in odorless mineral spiritsCAS Number: 19910-65-7Acrony..
One Hour Half Life Temperature 63.0 °C
145 °F
Akzo Nobel Trigonox® SBP-W50 Polymerization Initiator
Initiator for the (co)polymerization of vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonate, 50% emulsion in water and methanolCAS Number: 19910-65-7Acronym: SBP..