Polymer Property : Particle Mesh Size = 230 Mesh Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Mesh Size 230 Mesh
230 Mesh
5%; Geon® 812
PolyOne Geon™ 140 Series 140X466 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin..
Particle Mesh Size 230 Mesh
230 Mesh
5%; Geon® 812
PolyOne Geon™ 140 Series 140X484 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin..
Particle Mesh Size 230 Mesh
230 Mesh
5%; Geon® 812
PolyOne Geon™ 140 Series 140X497 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin..
Particle Mesh Size 230 Mesh
230 Mesh
Minimum of 70%
H.C. Starck Amperweld® 1701.39 K2 Chromium Carbide RIII
HS Number: 284990
Particle Mesh Size 230 Mesh
230 Mesh
Minimum of 85%
H.C. Starck Amperweld® 1701.39 K3 Chromium Carbide RIII
HS Number: 284990
Particle Mesh Size 230 Mesh
230 Mesh
screening fraction max 0.5%; Sieve Analysis per ASTM B214
H.C. Starck MoMP 3.5 - 4.5 micron Molybdenum Metal Powder, Mo (99.95%)
Description of Product: Grey metal powder. Sieved.Typical Applications: The production of pressed and sintered Mo or Mo alloy parts. Also used to produce blended alloy powders.Information provid..
Particle Mesh Size 230 Mesh
230 Mesh
screening fraction max 0.5%; Sieve Analysis per ASTM B214
H.C. Starck MoMP 4.5 - 5.5 micron Molybdenum Metal Powder, Mo (99.95%)
Description of Product: Grey metal powder. Sieved.Typical Applications: The production of pressed and sintered Mo or Mo alloy parts. Also used to produce blended alloy powders.Information provid..
Particle Mesh Size 230 Mesh
230 Mesh
Opening 1700µm; ASTM E11
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS
Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th..