Physical Properties Metric English Comments
Particle Mesh Size 20 - 30 Mesh
20 - 30 Mesh
US Sieve
Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..