Polymer Property : Surface Tension = 17.8 dynes/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Surface Tension 17.8 dynes/cm
17.8 dynes/cm
Dow Corning XIAMETER® PMCPPMX-0244 Cyclotetrasiloxane
Is chemically equivalent to DOW CORNING® 244 FLUID. This product is a volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension and evaporates completely at room..