Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 41 dynes/cm | 41 dynes/cm | 25°C |
LyondellBasell Propylene Carbonate Information provided by Lyondell. |
|||
Surface Tension | 41 dynes/cm | 41 dynes/cm | |
Solvay RHODASURF® B1 Surfactant Identification: ETHOXYLATED FATTY ALCOHOLCAS: 68551 – 12 – 2Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApp.. |