Physical Properties Metric English Comments
Surface Tension 55 - 60 dynes/cm
55 - 60 dynes/cm
Method L-005/L-040; ASTM D1417
Nitriflex Nitrilatex L-2108 Styrene Butadiene Latex
NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® HD-1800 HDPE
Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® KF Aramid Fiber Pulp
Product Description: INHANCE KF fiber is an aramid fiber pulp that has been surface activated by a proprietary reactive gas process. Surface activation makes the fibers easy to disperse, and create..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® PEF High Density Fibrillated Polyethylene
Product Description: INHANCE PEF fiber is a high density fibrillated (highly branched) polyethylene fiber that has been surface activated by a proprietary reactive gas process. Surface activation m..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® UH-1250 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® UH-1700 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® UH-1900 Ultra High Molecular Weight Polyethylene
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse..
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable
Inhance Fluoro-Seal INHANCE® HD-1035 HDPE
Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to..