Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 71.5 dynes/cm | 71.5 dynes/cm | |
BASF Hexamethylenediamine Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF |