Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 140 - 180 g/10 min

@Load 21.6 kg,
Temperature 180 °C
140 - 180 g/10 min

@Load 47.6 lb,
Temperature 356 °F
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..