Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 2.2 - 2.8 g/10 min @Load 21.6 kg, Temperature 190 °C |
2.2 - 2.8 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GV 0350 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |