Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 7.0 g/10 min @Load 21.6 kg |
7.0 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
High Load Melt Index | 7.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
High Load Melt Index | 7.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem HB 0155 HDPE Blow Molding Polyethylene Applications: Large containers from 60 to 200 litersInformation provided by Braskem |
|||
High Load Melt Index | 7.0 g/10 min @Load 21.6 kg, Temperature 250 °C |
7.0 g/10 min @Load 47.6 lb, Temperature 482 °F |
|
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced General-purpose grade with 30% glass fiber for parts requiring especially good resistance to heat deformation.Applications: parts for hot-water contact, pump housings, fan blades.Data was collected .. |
|||
High Load Melt Index | 7.0 g/10 min @Load 21.6 kg, Temperature 260 °C |
7.0 g/10 min @Load 47.6 lb, Temperature 500 °F |
|
Ashley Polymers Ashlene® PC/ABS Alloy 307WO General purpose flame retardant with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |
|||
High Load Melt Index | 7.0 g/10 min @Load 21.6 kg, Temperature 260 °C |
7.0 g/10 min @Load 47.6 lb, Temperature 500 °F |
|
Ashley Polymers Ashlene® PC/ABS Alloy 307 General purpose with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |