Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | <= 7.84 g/10 min @Load 20.0 kg, Temperature 260 °C |
<= 7.84 g/10 min @Load 44.1 lb, Temperature 500 °F |
4 mm; Non-standard Test |
Nanocyl PLASTICYL™ HDPE1501 High Density Polyethylene - Carbon Nanotube Masterbatch PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |