Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.500 - 0.720 mm | 0.0197 - 0.0283 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.500 - 0.720 mm | 0.0197 - 0.0283 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-401 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.500 - 0.720 mm | 0.0197 - 0.0283 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.500 - 0.720 mm | 0.0197 - 0.0283 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-401 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |