Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.36 - 1.74 mm | 0.0535 - 0.0685 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-100H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 1.36 - 1.74 mm | 0.0535 - 0.0685 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 1.36 - 1.74 mm | 0.0535 - 0.0685 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-101 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Bead Size | 1.36 - 1.74 mm | 0.0535 - 0.0685 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-100H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 1.36 - 1.74 mm | 0.0535 - 0.0685 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 1.36 - 1.74 mm | 0.0535 - 0.0685 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-101 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |