Polymer Property : Bead Size = 0.710 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 0.400 - 0.710 mm
0.0157 - 0.0280 in
IRPC Polimaxx Pentfoam 455E Expandable Polystyrene
GENERAL: PENTFOAM "455E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST CYCLES IN VACUUM MOL..