Physical Properties Metric English Comments
Bead Size 1.40 - 2.40 mm
0.0551 - 0.0945 in
Ineos Nova T243C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
Bead Size 1.40 - 2.50 mm
0.0551 - 0.0984 in
BASF Neopor® 2200 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..