Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 180 cm³/g | 180 cm³/g | Viscosity Number |
DSM Akulon® S227-C Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Viscosity Test | 180 cm³/g | 180 cm³/g | Viscosity Number |
DSM Stanyl® TE373 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Viscosity Test | 180 cm³/g | 180 cm³/g | Viscosity Number |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Viscosity Test | 180 cm³/g | 180 cm³/g | Viscosity Number |
Arkema Group Lacovyl® PB 1704 H PVC LACOVYL PB 1704 H is a vinyl chloride homopolymer manufactured by microsuspension polymerization process for the preparation of plastisols.It is specially designed for compact articles with low plas.. |