Polymer Property : Viscosity Test = 244 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 244 cm³/g
244 cm³/g
Viscosity Number
DSM Akulon® F236-C Nylon 6 (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..