Polymer Property : Viscosity Test = 58 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® 24 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® 24 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® 24 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® F 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® FC 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® F 23 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® FC 23 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 58 cm³/g
58 cm³/g
Viscosity Number
Mitsubishi Xantar® MX 2015 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..