Physical Properties Metric English Comments
Viscosity Test 66 cm³/g
66 cm³/g
Viscosity number
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.