Polymer Property : ESCR 100% Igepal® = 10 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 100% Igepal® <= 10 hour
<= 10 hour
Condition B; ASTM D 1693
NOVA Chemicals Sclair® IG454-A Compression Molded HDPE Resin
IG454-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG454..
ESCR 100% Igepal® <= 10 hour
<= 10 hour
Condition B, F50; ASTM D1693
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding
This hexene copolymer is tailored for injection molded applications that require:Excellent flowModerate impact strengthGood stiffnessTypical injection molded applications for 9035 include items such..
ESCR 100% Igepal® 10 hour
10 hour
ASTM D1963
ExxonMobil HDPE AP60-007 High Density Polyethylene Resin
Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
ESCR 100% Igepal® 10 hour
10 hour
F50; ASTM D1963A
ExxonMobil HDPE HD 8760.29 High Density Polyethylene Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
ESCR 100% Igepal® 10 hour
10 hour
F50; ASTM D1963A
ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
ESCR 100% Igepal® 10 hour
10 hour
ASTM D1693 Condition B
ExxonMobil Paxon™ AD60-005 Blow Molding Resin
Product Description: AD60-005 is a medium molecular weight districution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
ESCR 100% Igepal® 10 hour

@Temperature 50.0 °C
10 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-8335 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow
ESCR 100% Igepal® 10 hour
10 hour
ASTM D1693 Condition A
ExxonMobil HDP8760.29 Rotational Molding Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
ESCR 100% Igepal® 10 hour
10 hour
ASTM D1693 Condition B
ExxonMobil Paxon™ AD60-007 Blow Molding Resin
Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
ESCR 100% Igepal® 10 hour
10 hour
Bapolene® 0760 Polyethylene, Blow Molding Grade
This resin is a high density polyethylene homopolymer for blow molding applications. It is recommended for applications that require high top load strength and good stiffness. This product meets 2..
ESCR 100% Igepal® 10 hour
10 hour
ASTM D1693 Condition A
ExxonMobil HD 8760.29 Rotational Molding Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..