Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 139 hour @Thickness 2.00 mm, Temperature 50.0 °C |
139 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem GD5150K HDPE High Density Extrusion Polyethylene GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric.. |