Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | >= 160 hour | >= 160 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
ESCR 100% Igepal® | >= 160 hour | >= 160 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
ESCR 100% Igepal® | >= 160 hour | >= 160 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
ESCR 100% Igepal® | >= 160 hour | >= 160 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |