Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 46 hour @Thickness 2.00 mm, Temperature 50.0 °C |
46 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem HB0454 HDPE Blow Molding Polyethylene Copolymer HB0454 is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454 shows excellent processability, color, and superficial.. |